Project Description
FeNiCu Sealing Alloy
S4J47A
Equivalent Grades
GB | ГОСТ | ASTM | UNS | DIN | W.Nr. | NF | BS | JIS | SS |
S4J47A | 47НД | – | – | – | – | – | – | – | – |
Chemical Composition, %
Alloy | C | Mn | Si | P | S | Ni | Cu | Fe |
S4J47A | ≤0.05 | ≤0.4 | ≤0.3 | ≤0.015 | ≤0.015 | 46-48 | 4.5-5.5 | Rest |
Average Linear Expansion Coefficient
Alloy | Heat treatment for sample | Average linear expansion coefficient a/10-6.K-1 | Inflection point /℃ | ||
S4J47A | Heating to temperature between 850~900℃ in a protective or vacuum atmosphere. Holding for 1hour, cooling to 400℃ at a rate less than 300℃ per hour, then air cooling | 20~300℃ | 20~400℃ | 20~450℃ | ≥420 |
9.2~10.1 | 9.3~9.9 | 9.8~10.4 |
Available Products and Specifications
Rod, Bar, Wire and Forgings | ГОСТ 10994-1974, ГОСТ 14080-78 |
Plate, Sheet and Strip | ГОСТ 10994-1974, ГОСТ 14080-78 |
Pipe and Tube | ГОСТ 10994-1974, ГОСТ 14080-78 |
Welding Product | – |
Others | ГОСТ 10994-1974, ГОСТ 14080-78 |